Approve the colour separately on each material, against one physical reference, and give one person the final signature. A cotton polo, a polyester softshell, a screen print and an embroidery thread take colour in different ways, so at best they land close to each other. Your job is to decide how close is close enough for each item, and to do it before anything goes into bulk.
The differences have ordinary causes. Cotton and polyester are typically dyed with different dye types. Print ink sits on or near the surface and can be influenced by the garment colour underneath. Thread comes from a maker’s shade range and often has a sheen that changes with the angle, and a textured piqué reflects light differently from a smooth shell. When the mill, the maker and the decorator are three separate suppliers, each can honestly say its part matches while the set does not, and nobody owns the whole colour unless you name someone.
Fix the physical reference first
Brand guidelines usually quote a spot colour for print, and that is the wrong starting point for a mill. Pantone’s Formula Guide is its reference for graphics and print, shown on coated and uncoated paper stocks. Its textile system is separate. The Fashion, Home + Interiors guide uses paper TPG colours that Pantone says match back to its cotton TCX system, and the cotton swatch card is a piece of cotton poplin you can hold against a sample. That is a statement about Pantone’s own references and promises nothing about your fabric.
Polyester needs its own decision. Pantone’s polyester swatch card comes in 203 colours, which it describes as curated to represent the most sought-after shades, far fewer than the cotton card’s 2,801. The colour numbers and names on the two product pages mostly differ, so your colour may have no polyester reference at all. Check the range first, and if it has none, judge polyester lab dips against the cotton card and record that decision.
So do this once, and write the result down. Lay the printed guideline colour beside the textile references under your agreed light, choose the closest, and buy a swatch as the programme’s master. Date it, keep it out of the light, and give each supplier its own swatch or an approved cutting. Light and handling can change a swatch, and your master is only useful while it stays stable.
Who approves what, and in what order
Name one colour approver on your side for the whole table, usually the brand lead. Everyone else submits to that person.
| Stage | What is being approved | Who supplies the proof | Judged against | Who signs |
|---|---|---|---|---|
| 1. Master | The textile swatch chosen from the guidelines | Your side | Guideline colour, in the agreed light | Colour approver |
| 2. Lab dip | The shade on each fabric quality, ideally with two or three options | Mill, through the maker | Master | Colour approver |
| 3. Bulk fabric | A cutting from each dye lot, before garments are cut | Mill or maker | Approved lab dip | Maker’s quality check, then you if close to the limit |
| 4. Strike-off | Each print method on the real fabric, in each garment colour | Decorator | Master, beside the approved fabric | Colour approver |
| 5. Thread sew-out | A named thread shade stitched on the real fabric | Decorator | Master, beside the strike-off | Colour approver |
| 6. Set check | One of everything, laid together | Whoever holds all the parts | The master, and each other | Colour approver, final |
| 7. Reorder | A new dye lot, thread batch or ink mix | The supplier making it | Retained standard for that material | Colour approver or named deputy |
Judge each proof against the master as well as the previous proof, because small differences can add up along a chain. Send the decorator your approved fabric or the garment itself, since a print approved on a look-alike ground may shift on the real one. Run the set check before the whole order is committed, because stages 2 to 5 can each pass while the finished set still looks wrong together. Choosing between print and embroidery comes before all this, and the method guide covers it.
How close, and under which light
For fabric against fabric, you can put a number on it. ISO 105-J03 gives a way to calculate colour difference, ΔEcmc(l:c), between two specimens of the same material measured under the same conditions, and allows you to specify a maximum for the closeness your end use needs. The two words to notice are “same material”. That suits a bulk lot checked against its approved lab dip. It does not suit a polo against a softshell, or a thread against a print, and those need a visual decision recorded at stages 4 to 6.
The abstract gives no universal limit and going further means buying the standard, so ask the mill or test laboratory what figure it can hold on that fabric and colour. A clause might read: “Bulk fabric against approved lab dip, same fabric: ΔEcmc(l:c) not above [agreed value], using ratio [agreed], measured under [agreed illuminant].”
Then fix the light. ISO/CIE 11664-2 defines illuminant D65 as representing average daylight, at about 6,500 K, and illuminant A as typical tungsten-filament lighting. An illuminant is a defined description of light, so a window or a tube sold as daylight is not the same thing. Ask what source the mill or laboratory uses, and have every proof judged in that light plus the light the garment will actually be seen in, such as a showroom or a shop floor. Two shades that agree in one light can differ in another. This effect, metamerism, is a particular risk when the samples use different dyes or fibres, as a mixed set does.
ISO 3664 sets viewing conditions for prints and transparencies and says it does not apply outside graphic technology and photography. It can apply to a paper proof of your artwork. Do not cite it for fabric shade approval, and ask the laboratory which viewing method it follows for textiles.
A hypothetical set, and where to accept a near match
The company, garments and decisions below are invented, and the acceptance choices are one reasonable set of judgements. The brand colour is a saturated teal, given in the guidelines as a coated spot colour. The order is a cotton piqué polo, a polyester softshell, a screen-printed T-shirt for events and an embroidered chest logo on the polo and softshell.
| Item | How the colour gets there | Realistic aim | Would accept | Would reject |
|---|---|---|---|---|
| Polo, cotton piqué | Dyed to order, lab dip against the master | Close visual match, as it is the largest area and sets the look | A slightly lighter or darker result if the hue holds | Any visible lean towards green or blue |
| Softshell, polyester | Nearest stock shell, because the quantity falls below the dyeing minimum | Same colour family beside the polo | A deeper, smoother look from the different surface | A shell that looks like a second brand colour when worn with the polo |
| T-shirt, screen print | Ink mixed for this job, strike-off on the real T-shirt | Close to the master on a white ground | A small drift, since this item is seldom seen beside the polo | Ink that changes hue between the garment colours ordered |
| Chest logo, embroidery | Nearest shade on the thread maker’s card, sewn on polo and softshell | Reads as the same logo at normal viewing distance | Sheen that looks lighter at some angles | A thread closer to another colour in the brand palette |
The ranking follows from how the items are seen. Polo and softshell appear on the same person, so they get the tightest attention. The event T-shirt is rarely beside either, so it can be more relaxed. Dyeing the softshell fabric or the thread to order could close the gap further, but minimums set by fabric and dye lot can make that poor value on a short run. Decide in advance whether you would rather go slightly lighter or slightly darker, since a difference in depth is often easier to live with than a change in hue.
Holding the colour on a reorder
An approval speaks only for the swatch or proof in front of you, so the reorder needs physical evidence. Keep dated, labelled pieces out of the light:
- the approved lab dip and a cutting from the first bulk lot, per fabric
- the signed strike-off, per print method and garment colour, with whatever mixing reference the decorator will share
- the signed sew-out, with the thread maker and shade number
- the set-check photographs, as a reminder only, since a photograph is a poor guide to colour
A new dye lot gets compared with the retained standard, and the same goes for a new thread batch or ink mix. A new decorator or mill starts again from the physical standard, with a fresh strike-off or lab dip. Stock fabrics can drift between batches too, so ask to see a current cutting before reordering.
Colours can also move apart in use. If the polo goes through a hot laundry and the softshell does not, they may age differently, and colour fastness testing is a separate check from anything above. If the set has to stay matched for years, wash a pair of approved samples through your real route and look at them side by side.
On a mixed set, tell Dessa Textile which item carries the colour and what physical reference you hold.