“100% cotton single jersey, 160 g/m²” is not yet a fabric specification. Two jerseys with that label can use different yarns, different loop sizes and different finishing routes, and they will print, wear, shrink and twist differently. If you are buying T-shirts under your own label, the decision is which of those variables you fix in writing: yarn count and type, the loop density of the finished fabric, the finishing route, and tested targets for shrinkage and spirality, all checked on a sample before bulk.
Four variables that a fabric name hides
A T-shirt fabric is the result of four separate choices, and each one can change without the others.
- Fibre: what the yarn is made of, here cotton. Fibre quality and preparation (carded or combed) affect the yarn that can be spun from it.
- Yarn: how the fibre is spun and how fine it is. The yarn count states fineness, the spinning system (ring, compact, open-end) and the twist shape its behaviour, and a yarn can be single or plied.
- Construction: how the yarn is turned into fabric. Single jersey is one specific weft-knitted structure; piqué or interlock made from the same yarn behave differently.
- Finish: what happens after knitting: preparation, dyeing, drying, relaxation, compaction or chemical finishing.
GSM is an outcome of all four, not a fifth variable you can order independently. Our guide to reading GSM on a quotation explains why the figure alone says nothing about durability, quality or warmth.
How single jersey is built
Knits are made by intermeshing yarn into loops. In single jersey, every needle knits a plain loop in every course, so all loops look alike. CottonWorks describes the basic structure this way: the horizontal row of loops formed across the fabric is a course, and the vertical column of loops is a wale. Each loop has two legs and a crown. On the technical face you mainly see the legs, which form a V and give the smooth vertical surface usually printed on; on the technical back you see the crowns, which look like small horizontal arcs.
Two consequences matter for a garment. First, according to CottonWorks’ page on single and double knits, jersey stretches roughly twice as much across the width as along the length, and its cut edges curl. That is why cutting, neck binding and hem construction have to suit the fabric. Second, single jersey is usually knitted on circular machines, which build the fabric as a spiral tube; the number of needles sets the width of the tube, and one revolution makes one course per yarn feeder. That spiral is one root of the twisting described below.
The length of yarn in one loop is the loop length, also called stitch length. CottonWorks defines it as the course length divided by the number of needles used. A shorter loop gives a tighter fabric, a longer loop a looser one. Loop length is the main lever a knitter has, and it ties yarn, density and weight together.
Same GSM, different fabric
Weight per square metre is simply the number of loops in a square metre multiplied by the yarn in each loop and by the mass of that yarn. With loops per square centimetre (S), loop length in millimetres (ℓ) and yarn linear density in tex (grams per 1,000 metres):
GSM = S × ℓ × tex ÷ 100
Cotton yarns are usually traded in English count (Ne), where a higher number means a finer yarn; CottonWorks gives the conversion tex = 590.6 ÷ Ne. The table below is a hypothetical calculation, not a fabric recipe and not an offer from any mill. It shows how three different combinations arrive at the same 150 g/m².
| Hypothetical variant | Yarn | Linear density | Loop length | Loops per cm² needed for 150 g/m² | What differs |
|---|---|---|---|---|---|
| A, reference | Ne 30/1 | 19.7 tex | 2.75 mm | about 277 | Starting point for comparison |
| B, coarser yarn | Ne 24/1 | 24.6 tex | 3.05 mm | about 200 | Fewer, larger loops; more open structure; coarser yarn is usually cheaper per kilogram |
| C, finer yarn | Ne 34/1 | 17.4 tex | 2.55 mm | about 338 | More, smaller loops; finer surface; finer yarn costs more |
Check the arithmetic: 277 × 2.75 × 19.7 ÷ 100 ≈ 150, 200 × 3.05 × 24.6 ÷ 100 ≈ 150 and 338 × 2.55 × 17.4 ÷ 100 ≈ 150. Whether a real fabric settles at those densities depends on the machine, the yarn and the finishing route; that is the mill’s engineering, and the figures here only show the principle.
What a buyer should take from it: if you specify GSM alone, a supplier can meet it with variant A, B or C, and you would get a different T-shirt each time. Cotton Incorporated’s bulletin on wet processing of cotton knits adds two points that make this concrete. The machine gauge limits which yarn counts can be knitted on it, and for any given yarn count a smaller loop gives a heavier, more stable fabric. A shorter loop also reduces length shrinkage but raises width shrinkage at a specified finished width. So yarn, loop and width have to be agreed together, and stating wale and course counts per centimetre on the finished fabric is the simplest way to pin the construction down.
Spirality: why side seams twist
Spirality, also called skew or torque, is the angular displacement of wales and courses from a right angle. On a T-shirt it shows as a side seam that walks towards the front or back after washing. Cotton Incorporated’s technical bulletin Knit Fabrics and the Reduction of Torque lists the causes it found in 100% cotton single jersey:
- Yarn twist level: in its trials, a higher twist multiple gave more skew.
- Twist direction: Z-twist yarns leaned the loops to the right, S-twist yarns to the left.
- Spinning system: in that comparison, open-end yarns skewed less than ring-spun or air-jet yarns.
- Stitch tightness: the tighter the stitch, the less the skew.
- Feeders and machine rotation: more yarn feeders make more course skew, and depending on the direction of the cylinder, the yarn’s skew and the machine’s skew can add up or partly cancel.
- Finishing: in its tests, resin finishing gave the best control. Fabric straightened during drying still skewed as much after washing as unstraightened greige fabric.
The bulletin’s most effective remedies were plied yarns or alternating feeds of S- and Z-twist yarn. On one 28-cut machine, skew after five home launderings fell from 15.3% with all-Z feeds to 1.4% with alternating feeds. These are research results under the bulletin’s own conditions, not values to expect from any particular fabric. The practical lesson is that spirality is decided in yarn and knitting and only partly managed in finishing; pulling the fabric straight on the cutting table does not remove it.
For tests, ISO 16322-2 covers spirality of fabrics after domestic laundering and ISO 16322-3 covers garments. Both scope notes say results from different procedures may not be comparable, and that circular-knitted fabrics can have an inherent non-vertical wale line. They are methods, not pass limits, so the acceptable value has to be agreed with the fabric supplier.
Shrinkage, relaxation and compaction
Cotton Incorporated’s shrinkage guide for sourcers splits shrinkage into two parts. Construction shrinkage comes from the yarn and knitting variables. Processing shrinkage is what dyeing, finishing and garment making add or remove, usually by stretching the fabric in length and narrowing it in width. The fabric’s relaxed dimensions, the state in which it will not shrink further in washing and tumble drying, are called the reference state. The guide also warns that some shrinkage specifications cannot be reached at all, and that consistency from garment to garment matters as much as the value.
Finishers have three main tools, described in the TRI 3011 bulletin and on CottonWorks’ shrinkage and skewing page:
- Relaxation drying: the wet fabric is dried on a belt without tension and with controlled overfeed, so it can shrink before it reaches you. Width usually shrinks first, so the width must be adjusted afterwards.
- Compacting: the course loops are pressed together mechanically with heat and moisture, using heated rolls or shoe or belt units. It is used mainly on tubular goods. The bulletin notes that too much silicone softener can prevent compaction or let it release during cutting and sewing.
- Chemical crosslinking (resin): used especially on open-width knits for low shrinkage without the extra bulk compaction gives, but the resin level has to be balanced against bursting strength.
None of these makes jersey shrink-proof. Agree a residual shrinkage target in length and width, and name the test: ISO 5077 describes how to determine dimensional change after a specified combination of washing and drying procedures, so the specification must also say which procedure and how many cycles. The garment pattern then needs a shrinkage allowance that matches the tested fabric.
What you can check yourself and what needs a laboratory
With a ruler, a pick glass and a scale you can check a lot at sample stage: which side is the technical face, whether the surface is even, finished width, wales and courses per centimetre (count over several centimetres, not one), and GSM with a circle cutter on conditioned fabric. You can also wash a garment at home and look at the side seams; that tells you something, but it is not a test result.
Loop length needs unravelling a counted number of loops, which a mill or laboratory does. Dimensional change and spirality to an ISO method, colour fastness and anything you want to put in a contract belong in a laboratory report on the same fabric quality, ideally from the production lot.
Writing single jersey into a T-shirt specification
At Dessa Textile we are a Slovak clothing manufacturer with production in Europe. We do not spin yarn or knit fabric; in garment production the jersey comes from knitting and dyeing mills, so the specification has to be written clearly enough to travel along that chain. We agree it in writing per quotation and approve a sample before bulk. A workable fabric section for a T-shirt tech pack states:
- fibre content, and combed or carded cotton if it matters to you;
- yarn count with unit (for example Ne or tex), single or plied, and spinning system;
- construction: single jersey, technical face as the outer side;
- finished GSM with an agreed tolerance and how it is measured;
- finished width and whether the fabric is tubular or open width;
- wales and courses per centimetre on the finished fabric;
- colour reference and dyeing route (piece-dyed, yarn-dyed or garment-dyed);
- finishing route: relaxation drying, compaction or resin, and any softener limits;
- dimensional change and spirality targets, with the test method and washing procedure;
- care instructions that match the procedure you tested.
The overall garment decisions, from fit to neck construction, are covered in our guide to T-shirt manufacturing.
Sample and bulk approval checklist
- Confirm that the sample fabric is the same quality as the bulk fabric: yarn, construction, finish and mill.
- Measure GSM, width and wale and course counts on the sample and record them as the reference.
- Wash one sample garment under the agreed procedure and check side-seam position, length and width.
- Ask for the fabric’s test report on dimensional change and spirality, and check the method and cycles named.
- Keep a sealed reference piece of approved fabric for bulk comparison.
- At bulk, recheck GSM and loop counts on fabric from the production lot, not only on the sample roll.
- For reorders, repeat the fabric quality code and finishing route rather than just the colour and weight.
Our article on moving from sample to bulk production explains how these checks fit into the wider approval sequence.
What drives price and minimum order
Fabric cost rises with finer and plied yarns, combed cotton, extra finishing steps such as compaction or resin, tighter dimensional targets that need more processing control, and dyeing to a specific colour. Testing adds cost and time. On our side, the minimum order is 300 pieces per style and colour, sampling takes about 10 business days and bulk production about 5 weeks, depending on product and quantity; fabric availability and the approvals above can move those dates, so they are planning figures, not guarantees. Each T-shirt programme is quoted separately for private label clothing.
Next step
If you are planning a T-shirt range, send us a request for quotation with the garment type, approximate quantity per style and colour, the fabric or a sample reference you want to match, and your target delivery date. We will come back with the questions that need settling before sampling.
Does a higher GSM mean a better T-shirt fabric?
No. The same weight per square metre can come from a fine yarn knitted in many small loops or a coarser yarn in fewer, longer loops. Those fabrics differ in surface, opacity, shrinkage behaviour and cost, so GSM has to be read together with yarn count, loop density and finishing.
Why do the side seams of some T-shirts twist after washing?
Usually because the single jersey skews as it relaxes. Cotton Incorporated research links the effect to yarn twist level and direction, the spinning system, how tight the stitch is, the number of yarn feeders on the knitting machine and the finishing route. It cannot be ironed out at the end; it has to be controlled in yarn, knitting and finishing.
Can shrinkage be removed completely from cotton jersey?
Not in practice. Knitted fabrics are more prone to dimensional change than wovens. Relaxation drying, compaction or chemical finishing reduce residual shrinkage, and the target should be agreed as a tested value under a named washing and drying procedure rather than as 'no shrinkage'.
What should a T-shirt fabric specification contain?
Fibre content, yarn count and type, the knitted construction, finished GSM and width, wale and course counts on the finished fabric, colour and dyeing route, finishing route, and dimensional-change and spirality targets with the test method that will be used to check them.
Sources
- Knit Basics, CottonWorks (Cotton Incorporated) (accessed )
- Single & Double Knits, CottonWorks (Cotton Incorporated) (accessed )
- Yarn Ply, Counts and Treatments, CottonWorks (Cotton Incorporated) (accessed )
- Shrinkage & Skewing, CottonWorks (Cotton Incorporated) (accessed )
- TRI 2002: Knit Fabrics and the Reduction of Torque, Cotton Incorporated (accessed )
- TRI 3011: Wet Processing of 100% Cotton Knitted Fabrics, Cotton Incorporated (accessed )
- ISP 1009: A Guide to Improved Shrinkage Performance of Cotton Fabrics, Cotton Incorporated (accessed )
- ISO 5077:2007 Textiles — Determination of dimensional change in washing and drying, ISO (accessed )
- ISO 16322-2:2021 Textiles — Determination of spirality after laundering — Part 2: Woven and knitted fabrics, ISO (accessed )
- ISO 16322-3:2021 Textiles — Determination of spirality after laundering — Part 3: Woven and knitted garments, ISO (accessed )